Abstract

ALNICO V is an oriented permanent magnet alloy. It has the highest energy product of all material. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on heat treating and machining. Filing Code: Fe-17. Producer or source: Indiana Steel Products Company. Originally published April 1960, revised September 1963.