Abstract

Aluminum C113 is an aluminum permanent mold casting alloy having good pressure tightness. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fatigue. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-129. Producer or source: Aluminum Company of America.