Abstract

Firthite-WF is a high-speed finish grade of titanium carbide cermet recommended for cutting tools for the machining of steel and some stainless steels. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on machining and joining. Filing Code: Ti-36. Producer or source: Firth Sterling Corporation.