Abstract

Nickel Copper Cast Alloy 410 is one of the most useful cast materials to withstand corrosives encountered in industry. It has tensile strength comparable to cast carbon steel and gives good performance under conditions of abrasion and erosion. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness and fatigue. It also includes information on low and high temperature performance, and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Ni-85. Producer or source: High alloy foundries.

This content is only available as a PDF.
You do not currently have access to this content.