Abstract

JESSOP-SAVILLE G.32 is a cobalt-base alloy having high oxidation and corrosion resistance. It is recommended for high temperature applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Co-21. Producer or source: Wm. Jessop & Sons Ltd. Originally published June 1960, revised June 1963.