Abstract
Silvan Star is a water hardening high-carbon tool steel recommended for general applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-130. Producer or source: Firth Sterling Corporation.