Abstract

Riverside No. 105 is a copper-base alloy having good spring strength and high electrical conductivity in the cold rolled condition. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Cu-136. Producer or source: H. K. Porter Company Inc..