Abstract

Carpenter Hi-Shock 60 is an air-hardening tool steel for tools and dies which require extreme shock resistance with tensile strengths over 350,000 psi. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, and machining. Filing Code: TS-139. Producer or source: Carpenter.