ENDURO 18-8STi is the titanium-type 304 stainless steel stabilized by titanium. It is not made sensitive to intergranular corrosion by heating within the carbide precipitation range. It is recommended for use at temperatures up to 1600 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-149. Producer or source: Republic Steel Corporation.