Amphos is a phosphorized oxygen-free copper having free-scaling properties, freedom from hydrogen embrittlement, improved cold workability, and desirable high softening temperature. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on forming, heat treating, and joining. Filing Code: Cu-135. Producer or source: American Metal Climax Inc..