HAYNES Alloy Cb-752 is a columbium-base alloy having good high temperature characteristics. It has 25,000 psi ultimate strength at 2400 F. It is recommended for space vehicles and nuclear reactors. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and shear andbearing strength as well as creep. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: Cb-6. Producer or source: Union Carbide Corporation, Stellite Division.