Hi-Wear 64 is a cold work tool steel offering improved wear resistance and low temperature heat treatment. It is a deep hardening non-deforming steel recommended for tools to blank and form abrasive materials. This datasheet provides information on composition, physical properties, and hardness. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-122. Producer or source: Carpenter.