Abstract

Boron Stainless Steel is a wrought austenitic alloy serving the atomic energy field in vital reactor shielding and control applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-135. Producer or source: Superior Steel Corporation.