Abstract
Kentanium K162B is a titanium carbide cermet having high heat and oxidation resistance along with high hardness and abrasion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness, creep, and fatigue. It also includes information on high temperature performance and corrosion resistance as well as machining and joining. Filing Code: Ti-33. Producer or source: Kennametal Inc..
abrasive wear resistance, chemical composition, compressive strength, corrosion-resistant alloys, creep properties, elasticity, fatigue properties, fracture toughness, hardness, heat resistance, high-temperature alloys, joinability, Kentanium K162B, machinability, oxidation resistance, physical properties, tensile properties
This content is only available as a PDF.
Copyright © ASM International® 1996
1996
ASM International
Topics
Corrosion-resistant alloys
High-temperature alloys
Titanium alloys
Chemical composition
Oxidation resistance
Joinability
Machinability
Compressive strength
Creep properties
Elastic modulus
Fatigue properties
Fracture toughness
Abrasive wear resistance
Hardness
Tensile properties
Physical properties
Thermal resistance
You do not currently have access to this content.