Abstract

ALMAG 35 is a high purity aluminum alloy of the aluminum-magnesium type which possesses high and stable combination of strength, shock resistance, and ductility in the cast condition. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-4. Producer or source: William F. Jobbins Inc.. Originally published January 1953, revised March 1962.