Abstract
REVERE No. 454 is a manganese bronze having high tensile strength and good corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: Cu-123. Producer or source: Revere Copper and Brass Inc..