Abstract

Nickel-200 is a wrought metal combining excellent mechanical properties with corrosion resistance. It retains its strength to an excellent degree at high temperatures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on low and high temperature performance, and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-75. Producer or source: Huntington Alloy Products Division.