Cupron is a copper-nickel resistance alloy recommended for maximum operating temperature of 1000 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. Filing Code: Cu-121. Producer or source: Wilbur B. Driver Company.