TORMANC SPECIAL is a low-carbon manganese-nickel-molybdenum steel for locomotive parts, railway and general engineering purposes. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-124. Producer or source: Samuel Fox & Company Ltd, Stocksbridge Works.