Abstract

BRIDGEPORT 712 is a highly corrosion resistant aluminum-silicon bronze having good spring characteristics. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-13. Producer or source: Bridgeport Brass Company. Originally published December 1953, revised January 1962.