Abstract
Mueller 602 is a bearing alloy possessing good machinability for use with hard or soft mating members where moderate strength will suffice. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, machining, and joining. Filing Code: Cu-106. Producer or source: Mueller Brass Company.