Abstract

Alten 50 WR is a low alloy cast iron recommended for high strength and pressure tight castings. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on heat treating, machining, and joining. Filing Code: CI-30. Producer or source: Alten Foundry & Machine Works Inc..

This content is only available as a PDF.
You do not currently have access to this content.