Climelt Molybdenum-0.5% Ti is a molybdenum alloy having high strength at elevated temperatures, high modulus of elasticity, low coefficient of expansion, and high thermal conductivity. It has exceptionally high rupture properties above 1600 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Mo-2. Producer or source: Climax Molybdenum Company.