Abstract

AISI 4650 is an oil hardening, medium-carbon alloy steel having high mechanical properties, endurance limit and shock resistance. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: SA-121. Producer or source: Alloy steel mills and foundries.